| dc.description.abstract | Pnictogen chalcohalides (MChX) have recently emerged as promising nontoxic and environmentally friendly photovoltaic absorbers, combining strong light absorption coefficients with favorable low-temperature synthesis conditions. Despite these advantages and reported optimized morphologies, device efficiencies remain below 10%, far from their ideal radiative limit. To uncover the origin of these performance losses, we present a systematic and fully consistent first-principles investigation of the defect chemistry across the Bi-based chalcohalide family. Our results reveal a complex defect landscape dominated by chalcogen vacancies of low formation energy, which act as deep nonradiative recombination centers. Despite their moderate charge-carrier capture coefficients, the high equilibrium concentrations of these defects reduce the theoretical maximum efficiencies by 6% in BiSeI and by 10% in BiSeBr. In contrast, sulfur vacancies in BiSI and BiSBr are comparatively benign, presenting smaller capture coefficients due to weaker electron-phonon coupling. Interestingly, despite its huge nonradiative charge-carrier recombination rate, BiSeI presents the best conversion efficiency among all four compounds owing to its most suitable bandgap for outdoor photovoltaic applications. Our findings identify defect chemistry as a critical bottleneck in MChX solar cells and propose chalcogen-rich synthesis conditions and targeted anion substitutions as effective strategies for mitigation of detrimental vacancies. | * |
| dc.language | English | * |
| dc.publisher | AMER CHEMICAL SOC | * |
| dc.title | Defect-Limited Efficiency of Pnictogen Chalcohalide Solar Cells | * |
| dc.type | Article | * |
| dc.relation.issue | 6 | * |
| dc.relation.volume | 38 | * |
| dc.relation.index | SCIE | * |
| dc.relation.index | SCOPUS | * |
| dc.relation.startpage | 2893 | * |
| dc.relation.lastpage | 2903 | * |
| dc.relation.journaltitle | CHEMISTRY OF MATERIALS | * |
| dc.identifier.doi | 10.1021/acs.chemmater.5c03275 | * |
| dc.identifier.wosid | WOS:001696682300001 | * |
| dc.identifier.scopusid | 2-s2.0-105033826642 | * |
| dc.author.google | Lopez, Cibran | * |
| dc.author.google | Kavanagh, Sean R. | * |
| dc.author.google | Benitez, Pol | * |
| dc.author.google | Saucedo, Edgardo | * |
| dc.author.google | Walsh, Aron | * |
| dc.author.google | Scanlon, David O. | * |
| dc.author.google | Cazorla, Claudio | * |
| dc.contributor.scopusid | Aron Walsh(35315151400) | * |
| dc.date.modifydate | 20260813144119 | * |